EN 12697-17:2026
(Main)Bituminous mixtures - Test methods - Part 17: Particle loss of porous asphalt specimens
- Abstract
This document specifies a test method for determining the particle loss of porous asphalt mixtures. Particle loss is assessed by the loss of mass of porous asphalt samples after turns in the Los Angeles machine. This test enables the estimation of the abrasion resistance of porous asphalt. The test applies to laboratory compacted cylindrical specimens of porous asphalt mixtures, the upper sieve size of which does not exceed 22,4 mm. It does not reflect the abrasive effect by studded tyres.
- Status
- Not Published
- Publication Date
- 22-Dec-2026
- Technical Committee
- CEN/TC 227 - Road materials
- Drafting Committee
- CEN/TC 227/WG 1 - Bituminous mixtures
- Current Stage
- 5060 - Closure of Vote - Formal Approval
- Start Date
- 05-Nov-2026
- Due Date
- 06-Apr-2026
- Completion Date
- 05-Nov-2026
EN 12697-17:2026 is a CEN standard for testing porous asphalt specimens. It specifies a Los Angeles machine method for measuring particle loss from laboratory compacted cylindrical porous asphalt specimens with an upper sieve size not exceeding 22,4 mm. The result is used to estimate abrasion resistance, and the method does not represent wear from studded tyres.
What does EN 12697-17:2026 specify?
EN 12697-17:2026 specifies one test method for particle loss of porous asphalt mixtures and shows how to report the result. The document is organized into scope, normative references, terms and definitions, apparatus, specimen preparation, procedure, calculation, test report, precision, and an informative annex on water conditioning.
The main body covers the standard dry test. Annex A adds a comparison between air-dried and water-immersed specimens, which is useful when assessing the effect of moisture on particle loss.
| Annex | What it covers |
|---|---|
| Annex A (informative) | Effect of water on particle loss of porous asphalt specimens, including the comparison between dry and wet conditioning and the increase in particle loss |
What are the key requirements of EN 12697-17:2026?
EN 12697-17:2026 is built around a controlled specimen preparation, a defined Los Angeles machine procedure, and a mass-loss calculation. In practice, the reader needs to prepare comparable specimens, control temperature and conditioning time, and report the average result for five tests.
Specimen preparation
Clause 5 requires at least five specimens per sample and condition. The specimens are cylindrical, laboratory compacted, and measured to the dimensions given in the document: diameter and height are controlled, and their bulk density and void content are determined before testing. This matters because specimen size, density, and voids influence the test result.
Clause 5 also requires storage before testing for a defined period at not more than 25 °C. The note explains that storage time can affect mechanical properties, so the age of the specimen has to be controlled and reported.
Apparatus and temperature control
Clause 4 specifies the Los Angeles machine, thermometer, chamber or room, oven, and balance. The thermometer and balance have defined permissible errors, and the test environment must hold the specimen and machine at the required temperature range. This matters because particle loss is sensitive to temperature and weighing accuracy.
Test procedure
Clause 6 requires the specimen to be conditioned at the test temperature before testing. The usual test range is 15 °C to 25 °C, with lower local temperatures allowed for cold climate zones. The specimen is then turned in the Los Angeles machine without the metal balls, at 30 rpm to 33 rpm for 300 turns, and weighed before and after the test.
The clause also notes that loose particles are lightly removed with a cloth before the final weighing. That means the result is based on particles that remain attached after the test, not on dust or loosely detached material already separated during handling.
Calculation and reporting
Clause 7 calculates particle loss from the change in specimen mass, then gives the result as the average of five single values, rounded to the nearest 1 %. In practice, this gives one reported particle-loss value for the sample and condition tested.
Clause 8 lists the information that has to appear in the test report: sample identification, reference to the document, test temperature, average particle loss, compaction method, specimen characteristics, age and storage conditions, deviations, and unusual observations. Those observations can help explain why one mixture performs better or worse.
Precision
Clause 9 gives repeatability and reproducibility data for results below 40 % and for results at or above 40 %. It also states the interlaboratory conditions used to establish those values. This helps laboratories judge whether two results are reasonably close.
What changed in EN 12697-17:2026 from the previous edition?
The foreword says this edition supersedes EN 12697-17:2017. It also states these changes:
- Clause 2: the series title is no longer exclusive to hot mix asphalt; EN 12697-29 is added and EN 12697-35 is removed.
- Subclause 4.2: the thermometer requirement changes from an accuracy statement to a maximum permissible error of 0,5 °C.
- Subclause 4.5: the balance requirement changes to readability of 0,1 g and a maximum permissible error of 1 g.
- Clause 5: specimen requirements are reworded and renumbered, and the requirements change from mass-based to dimension-based.
- Clause 5: the clause on asphalt with aggregate larger than 16 mm is deleted.
- Clause 6 and Clause 7: the mass symbol changes from W to m, and the speed text 3,1 rad/s to 3,5 rad/s is deleted.
- Clause 8: the test report information is reworded and renumbered.
- Annex A: a new informative annex is added on the effect of water on particle loss.
Which standards are used with EN 12697-17:2026?
EN 12697-17:2026 refers to these standards for equipment, specimen preparation, measurement, and precision work:
- EN 1097-2 - specifies the Los Angeles machine used in the test.
- EN 12697-5 - provides maximum density determination for the mixture.
- EN 12697-6 - provides bulk density determination of bituminous specimens.
- EN 12697-8 - provides void characteristics of bituminous specimens.
- EN 12697-29 - provides specimen dimension measurement.
- EN 12697-30 - provides specimen preparation by impact compactor.
- EN 12697-31 - provides specimen preparation by gyratory compactor.
- EN 12697-35 - is named for bituminous mixture preparation in Clause 5.
- ISO 5725 (all parts) - is used for the repeatability and reproducibility study cited in Clause 9 and Annex A.
What does the EN 12697-17:2026 document contain?
EN 12697-17:2026 contains the apparatus requirements, the specimen preparation rules, the test procedure, the mass-loss calculation, the reporting items, and the precision statement. It also includes an informative annex on how water conditioning affects particle loss.
The detailed parts specify the machine setup, temperature control, specimen dimensions, storage before testing, and the exact turning procedure in the Los Angeles machine. Annex A extends the method to wet conditioning and adds a calculation for the increase in particle loss due to water exposure.
The document also gives the content expected in the test report, so laboratories can document the sample, the compaction method, specimen characteristics, test temperature, deviations, and notable observations in a consistent way.
Relations
- Effective Date
- 21-Feb-2024
Get Certified
Connect with accredited certification bodies for this standard

Zavod za gradbeništvo Slovenije (ZAG) - Inšpekcija
ZAG inspection body for construction products, structures, and materials.
Sponsored listings
Frequently Asked Questions
EN 12697-17:2026 is a draft published by the European Committee for Standardization (CEN). Its full title is "Bituminous mixtures - Test methods - Part 17: Particle loss of porous asphalt specimens". This standard covers: This document specifies a test method for determining the particle loss of porous asphalt mixtures. Particle loss is assessed by the loss of mass of porous asphalt samples after turns in the Los Angeles machine. This test enables the estimation of the abrasion resistance of porous asphalt. The test applies to laboratory compacted cylindrical specimens of porous asphalt mixtures, the upper sieve size of which does not exceed 22,4 mm. It does not reflect the abrasive effect by studded tyres.
This document specifies a test method for determining the particle loss of porous asphalt mixtures. Particle loss is assessed by the loss of mass of porous asphalt samples after turns in the Los Angeles machine. This test enables the estimation of the abrasion resistance of porous asphalt. The test applies to laboratory compacted cylindrical specimens of porous asphalt mixtures, the upper sieve size of which does not exceed 22,4 mm. It does not reflect the abrasive effect by studded tyres.
EN 12697-17:2026 is classified under the following ICS (International Classification for Standards) categories: 93.080.20 - Road construction materials. The ICS classification helps identify the subject area and facilitates finding related standards.
EN 12697-17:2026 has the following relationships with other standards: It is inter standard links to EN 12697-17:2017. Understanding these relationships helps ensure you are using the most current and applicable version of the standard.
EN 12697-17:2026 is associated with the following European legislation: EU Directives/Regulations: 305/2011; Standardization Mandates: M/124. When a standard is cited in the Official Journal of the European Union, products manufactured in conformity with it benefit from a presumption of conformity with the essential requirements of the corresponding EU directive or regulation.
EN 12697-17:2026 is available in PDF format for immediate download after purchase. The document can be added to your cart and obtained through the secure checkout process. Digital delivery ensures instant access to the complete standard document.
Standards Content (Sample)
SLOVENSKI STANDARD
oSIST prEN 12697-17:2025
01-maj-2025
Bitumenske zmesi - Preskusne metode - 17. del: Obraba delcev poroznih asfaltnih
preskušancev
Bituminous mixtures - Test methods - Part 17: Particle loss of porous asphalt specimens
Asphalt - Prüfverfahren - Teil 17: Kornverlust von Probekörpern aus offenporigem
Asphalt
Mélanges bitumineux - Méthodes d’essai - Partie 17 : Perte de matériau des éprouvettes
d’enrobé drainant
Ta slovenski standard je istoveten z: prEN 12697-17
ICS:
93.080.20 Materiali za gradnjo cest Road construction materials
oSIST prEN 12697-17:2025 en,fr,de
2003-01.Slovenski inštitut za standardizacijo. Razmnoževanje celote ali delov tega standarda ni dovoljeno.
oSIST prEN 12697-17:2025
oSIST prEN 12697-17:2025
DRAFT
EUROPEAN STANDARD
prEN 12697-17
NORME EUROPÉENNE
EUROPÄISCHE NORM
March 2025
ICS 93.080.20 Will supersede EN 12697-17:2017
English Version
Bituminous mixtures - Test methods - Part 17: Particle loss
of porous asphalt specimens
Mélanges bitumineux - Méthodes d'essai - Partie 17 : Asphalt - Prüfverfahren - Teil 17: Kornverlust von
Perte de matériau des éprouvettes d'enrobé drainant Probekörpern aus offenporigem Asphalt
This draft European Standard is submitted to CEN members for enquiry. It has been drawn up by the Technical Committee
CEN/TC 227.
If this draft becomes a European Standard, CEN members are bound to comply with the CEN/CENELEC Internal Regulations
which stipulate the conditions for giving this European Standard the status of a national standard without any alteration.
This draft European Standard was established by CEN in three official versions (English, French, German). A version in any other
language made by translation under the responsibility of a CEN member into its own language and notified to the CEN-CENELEC
Management Centre has the same status as the official versions.
CEN members are the national standards bodies of Austria, Belgium, Bulgaria, Croatia, Cyprus, Czech Republic, Denmark, Estonia,
Finland, France, Germany, Greece, Hungary, Iceland, Ireland, Italy, Latvia, Lithuania, Luxembourg, Malta, Netherlands, Norway,
Poland, Portugal, Republic of North Macedonia, Romania, Serbia, Slovakia, Slovenia, Spain, Sweden, Switzerland, Türkiye and
United Kingdom.
Recipients of this draft are invited to submit, with their comments, notification of any relevant patent rights of which they are
aware and to provide supporting documentation.
Warning : This document is not a European Standard. It is distributed for review and comments. It is subject to change without
notice and shall not be referred to as a European Standard.
EUROPEAN COMMITTEE FOR STANDARDIZATION
COMITÉ EUROPÉEN DE NORMALISATION
EUROPÄISCHES KOMITEE FÜR NORMUNG
CEN-CENELEC Management Centre: Rue de la Science 23, B-1040 Brussels
© 2025 CEN All rights of exploitation in any form and by any means reserved Ref. No. prEN 12697-17:2025 E
worldwide for CEN national Members.
oSIST prEN 12697-17:2025
prEN 12697-17:2025 (E)
Contents Page
European foreword . 3
1 Scope . 4
2 Normative references . 4
3 Terms and definitions . 4
4 Apparatus . 4
5 Preparation of test specimens . 5
6 Procedure. 5
7 Calculation . 6
8 Test report . 6
9 Precision . 6
Annex A (informative) Effect of water on particle loss of porous asphalt specimens . 8
Bibliography . 11
oSIST prEN 12697-17:2025
prEN 12697-17:2025 (E)
European foreword
This document (prEN 12697-17:2025 has been prepared by Technical Committee CEN/TC 227 “Road
materials”, the secretariat of which is held by BSI.
This document is currently submitted to the CEN Enquiry.
This document will supersede EN 12697-17:2017.
prEN 12697-17:2025 includes the following significant technical changes with respect to
EN 12697-17:2017:
— [Clause 2] the series title no longer makes the method exclusive to hot mix asphalt. Addition of
EN 12697-29 and removal of EN 12697-35;
— [Subclause 4.2] “accuracy of ±0,5 °C” amended to read: maximum permissible error of 0,5 °C;
— [Subclause 4.5] “accuracy of ±0,1 %” amended to read: readable to 0,1 g and with a maximum
permissible error of 1 g;
— [Clause 5] rewording and renumbering of text. Test specimen requirements changed from mass to
dimensions. Deletion of Clause describing the use of asphalt with an aggregate size greater than
16 mm;
— [Clause 6] mass symbol changed from “W” to “m”. Deletion of text “3,1 rad/s to 3,5 rad/s”;
— [Clause 7] mass symbol changed from “W” to “m”;
— [Clause 8] rewording and renumbering of information for the test report;
— [Annex A]: addition of new informative Annex A on the effect of water on particle loss of porous
asphalt specimens.
oSIST prEN 12697-17:2025
prEN 12697-17:2025 (E)
1 Scope
This document specifies a test method for determining the particle loss of porous asphalt mixtures.
Particle loss is assessed by the loss of mass of porous asphalt samples after turns in the Los Angeles
machine. This test enables the estimation of the abrasion resistance of porous asphalt. The test applies to
laboratory compacted cylindrical specimens of porous asphalt mixtures, the upper sieve size of which
does not exceed 22,4 mm. It does not reflect the abrasive effect by studded tyres.
2 Normative references
The following documents are referred to in the text in such a way that some or all of their content
constitutes requirements of this document. For dated references, only the edition cited applies. For
undated references, the latest edition of the referenced document (including any amendments) applies.
EN 1097-2, Tests for mechanical and physical properties of aggregates - Part 2: Methods for the
determination of resistance to fragmentation
EN 12697-5, Bituminous mixtures - Test methods - Part 5: Determination of the maximum density
EN 12697-6, Bituminous mixtures - Test methods - Part 6: Determination of bulk density of bituminous
specimens
EN 12697-8, Bituminous mixtures - Test methods - Part 8: Determination of void characteristics of
bituminous specimens
EN 12697-29, Bituminous mixtures - Test methods - Part 29: Determination of the dimensions of a
bituminous specimen
EN 12697-30, Bituminous mixtures - Test methods - Part 30: Specimen preparation by impact compactor
EN 12697-31, Bituminous mixtures - Test methods - Part 31: Specimen preparation by gyratory compactor
3 Terms and definitions
No terms and definitions are listed in this document.
ISO and IEC maintain terminology databases for use in standardization at the following addresses:
— ISO Online browsing platform: available at https://www.iso.org/obp
— IEC Electropedia: available at https://www.electropedia.org/
4 Apparatus
4.1 Los-Angeles-machine, as specified in EN 1097-2.
4.2 Thermometer, capable of covering the test temperature range with a maximum permissible error
of 0,5 °C.
4.3 Chamber, room or enclosure, large enough to fit the Los-Angeles-machine and capable of
maintaining the test temperature ± 2 °C in the vicinity of the Los-Angeles-machine.
4.4 Oven, equipped with a closed ventilation system or a chamber fitted with a thermostatic control
to maintain the test temperature within ± 1 °C in the vicinity of the samples.
oSIST prEN 12697-17:2025
prEN 12697-17:2025 (E)
4.5 Balance, of suitable capacity for the mass to be weighed, readable to 0,1 g and with a maximum
permissible error of 1 g.
5 Preparation of test specimens
5.1 At least five specimens shall be prepared for each sample and condition tested.
5.2 The bituminous mixture for specimens shall be prepared in accordance with EN 12697-35.
5.3 The specimens shall be cylindrical moulded by laboratory compaction as specified in EN 12697-30
by applying 2 × 50 blows, or EN 12697-31 compacted by 40 gyrations.
NOTE The compaction method can have an influence on the result.
5.4 The cylindrical specimens shall have a diameter of (100 ± 3) mm and a height of (63,5 ± 2,5) mm.
Dimensions of each test specimen shall be measured in accordance with EN 12697-29.
For mixtures with a bulk density of approximately 2,0 Mg/m , specimens with a mass of (1,0 ± 0,2) kg
should comply.
5.5 After the specimens have been compacted and removed from the mould, their bulk density shall be
determined in accordance with EN 12697-6 (Procedure D: bulk density by dimensions). The maximum
density of the mixture shall be determined in accordance with EN 12697-5, and then the void content of
each specimen shall be determined in accordance with EN 12697-8.
NOTE The density of the specimens can affect the result because the mass of a specimen will influence the
impact force imparted on contact during the test, particu
...